The other day SWIM came across a new tech, by experimentation ( not research ), and wants to share...
Wile cleaning up the remains of SWIM’s evap dishes ( the bits that SWIM couldnt scrape off ) SWIM noticed that the solv used ( benzine ) wasn’t dissolving the material easily...after that he tried with the DCM and the material melted like butter...but the benzine that seemed useless to do the cleanning showed after evaporation much highter concentrations then the DCM wash that dissolved all the material from the same dish after the Benzine was tryed...
He noticed then that with certain solvents like benzine (not benzene) and he guesses Nafta too, the fats and oils wont disolve very easily but the goodies will .
So he though of taking an advantage of this fact and of the fact that every solvent disolvs less material if frozen, and got into experimentation...results : cristals made straight out of goo very easily and with almost no waste !
The other recristalizations and purification methods avaliable in this site are much more complete, professional an eficient and SWIM recomends them as best (MadMax’s rocks !), althougt SWIM recomends this method for the newbees that dont want to get into a second A.B. mess, but want’s his cristals... this method is not the best but a easy and quick way to go...
THEORY :
Basically the idea is to dissolve the goodies slowly on good amounts of room temperature weak solvent ( sory my ignorance but I dont know the right term for this kind of solvents ), instead of dissolving it in as little as possible warm strong solvents ( like the DCM).
This method will allow the easy separation of the goodies from the fat that will dissolve very slowly throgh the process releasing the goodies and staying behind... changing goo straight into criastals with no second a.b.'s .
And after that cristalyzing goodies straight in the freezer and air drying the ready cristais.
EQUIPMENT NEEDED :
- 3 vials
- 1 spatula
- less then 1litre of Benzine ( nafta will probably work )
- Drying agent
- Freezer
- Vent fan
METHOD :
1- Prepair your solvent with the drying agent.
2- Pour your goo in one of the vials.
3- Pour ~ 10 ml of the dried solv. per g of goo ( if using less than 5 g put 50 ml ).
4- Mix very vigorously whith the spatula for about 10-15 min.working the goo to dissolve into the Benzine. ( notice that the goo is going to start sticking to the botom of your vial ).
5- Pour the mixed solv. into another vial, waching so none of the goo came togheter with the solv.. You want only the translucent solvent in the other vial, but dont wory to much because the goo it’s likely to stay stuck in the initial vial.
6- Repeat process other 3 times placing all the 200 ml of shaken solv in the same vial.
7- Put your vial into the freezer whith some pvc film covering so no ice falls into the solv.
8- Repeat washing process 5 times and pour the other 250 ml shaken solv in the other clean vial avaliable.
9- Put into freezer covered as the other.
10- Wait for ~ 3-4 hrs, then pour the solvs off the vials away togheter.
11- Put the 2 vials full of cristals ( with no solv. ) back into the freezer for another 30 min.
12- Take the vials and put them out for drying in the fan ( hight spead, but wach out so no powder flys away )
13- And presto !!! One vial full whith white ass loosen powder cristals and another vial of yelowish crumbly cristals... ~ 85-98 % yield from goo’s weight ( depends on its concentration ).
If you like you can reduce the remaining 450 ml solv to 50 ml, wash again the rest of the goo remaining in the initial vial for a longer time and whith the 50ml solv. slytely warm ( 30 C) and then put into freezing and drying one more time...If you dont have much it’s worthed, but there will be very little left at this point...
The remains of the process will be almost NADA of a thick sticky brown material, that of course you can still smoke , but SWIM dont advise unless you have nothing else left...
Keep the Vibe
I hope this can help out some newbees as this site have always done to SWIM...Tks Rhodium...